SF-08-Cu36-Sn4-58 is a low-density iron-bronze sintered bearing material per AMES reference standard. Equivalent to MPIF FCTG-3604-K16. Combines iron strength with bronze's conformability and corrosion resistance.
| Element | Content |
|---|---|
| Fe | 54.2–62.0% |
| Cu | 34.0–36.0% |
| Sn | 3.5–4.5% |
| C | 0.5–1.3% |
| Other | ≤2.0% |
| Property | Value |
|---|---|
| Density | 5.6–6.0 g/cm³ |
| Radial Crushing Strength K | ≥110 MPa |
| Oil Content (min.) | 21% |
Comparable Standards: MPIF FCTG-3604-K16. Radial crushing strength K is the mandatory value per AMES reference standard. Oil content represents minimum values at corresponding density levels.